Raschig Group Synres-Almoco B.V. AMC 2567
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical properties and dimensional stability, excellent processability. Self-extinguishing (V-0/0,7 according to UL 94). Free of halogens and toxic heavy metals. Forms: Dustfree granulate packed in moisture resistant cartons. Standard bag size: 25 kg palletized in 500 kg loads. Processing: Injection/Transfer/Compression. Applications: ConnectorsBobbinsHousingsMounting platesInformation provided by the Raschig Group
| Available Properties |
- Specific Gravity
- Apparent Bulk Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Surface Resistance
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 100°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Shrinkage
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Water Absorption, max [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|