Raschig Group Synres-Almoco B.V. AMC 2568
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for solder baths, excellent processability in combination with very short cycle times, low mouldwear. Self-extinguishing (V-0/1,4 according to UL 94) - UL-listed in color blue. Free of halogens and toxic heavy metals. Forms:Dustfree granulate packed in moisture resistant cartons. Standard bag size: 25 kg palletized in 500 kg loads. Processing: Injection or Transfer. Applications: ConnectorsBobbinsHousingsMounting platesInformation provided by the Raschig Group
| Available Properties |
- Specific Gravity
- Apparent Bulk Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 100°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Shrinkage
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Water Absorption, max [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|