Raschig Group Synres-Almoco B.V. AMC 2573

 

Subcategory: Polyester, TS; Thermoset; Polymer

Material Notes:
Short glass fiber reinforced, inorganically filled UP molding compound in color RAL 7035. Very good mechanical strength, very good electrical properties and dimensional stability, high flame retardance in combination with low fume toxicity, out standing processability - optimized for automatic processing. Self-extinguishing (V-0/1.1 according to UL 94) Free of halogens and toxic heavy metals. Forms: Dustfree granulate packed in moisture resistant bags. Standard bag size: 25 kg palletized in 500 kg loads. Processing: Compression.

Applications:

  • Thermostat housings
  • Switch parts
  • Relays
  • Junction box for light-masts
  • Information provided by the Raschig Group

    Available Properties
    • Specific Gravity
    • Apparent Bulk Density
    • Linear Mold Shrinkage
    • Flexural Modulus
    • Flexural Strength
    • Charpy Impact Unnotched
    • Surface Resistance
    • Comparative Tracking Index
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Flammability, UL94
    • Shrinkage
    • Mold Temperature
    • Water Absorption, max [mg]
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。