Raschig Group Synres-Almoco B.V. AMC 2573
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: Short glass fiber reinforced, inorganically filled UP molding compound in color RAL 7035. Very good mechanical strength, very good electrical properties and dimensional stability, high flame retardance in combination with low fume toxicity, out standing processability - optimized for automatic processing. Self-extinguishing (V-0/1.1 according to UL 94) Free of halogens and toxic heavy metals. Forms: Dustfree granulate packed in moisture resistant bags. Standard bag size: 25 kg palletized in 500 kg loads. Processing: Compression. Applications: Thermostat housingsSwitch partsRelaysJunction box for light-mastsInformation provided by the Raschig Group
| Available Properties |
- Specific Gravity
- Apparent Bulk Density
- Linear Mold Shrinkage
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Surface Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Shrinkage
- Mold Temperature
- Water Absorption, max [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|