Raschig Group Synres-Almoco B.V. DAIP 6552
Subcategory: Diallyl Phthalate (DAP); Thermoset; Polymer
Material Notes: Glass fiber-reinforced and inorganically filled diallylisophthalate molding compound (DAIP) in various colors. Good mechanical strength together with retention of high electrical properties under hot humid conditions, long term retention of dimensional stability also under severe environmental conditions. Self-extinguishing. Free of toxic heavy metals. Forms: Low dust granulate packed in moisture resistant cartons. Standard carton size: 20 kg palletized in 600 kg loads.Applications: ConnectorsBobbinsPotentiometersSwitchesInformation provided by the Raschig Group
| Available Properties |
- Specific Gravity
- Apparent Bulk Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 100°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Oxygen Index
- Shrinkage
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Water Absorption, max [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|