Raschig Group Synres-Almoco B.V. MELOPLAS® MP 183
Subcategory: Thermoset; Polymer
Material Notes: Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 181, high surface hardness, good mechanical strength and heat resistance, good abrasion and UV stability. Self-extinguishing (V-0/1,6 according to UL 94), UL-listed in all colors. Free of halogens and toxic heavy metals. Supervised according ISO 14529-3, DIN 7708: MP 183, ISO 800: MPF C10, ISO 14529-3: MP (LD20+MD30) -(LD30+MD20). Forms: Low dust granulate packed in moisture resistant bags. Standard bag size: 25 kg palletized in 1.000 kg loads or big-bags. Processing: Injection and compression, Applications: Molded parts in electrical engineering. Information provided by the Raschig Group
| Available Properties |
- Specific Gravity
- Apparent Bulk Density
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Modulus of Elasticity
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 100°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Oxygen Index
- Shrinkage
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Glow Resistance, class-mm
- Glow-wire test, 960°
- Needle-flame test
- Water Absorption, max [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|