RedEye RPM Clear PolyJet Resin FC720 for Rapid Prototyping

 

Subcategory: Thermoplastic; Polymer

Material Notes:
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offers the best surface finish. These parts are built at a layer thickness of 16 microns (0.0006 inch or 0.01524mm) and can produce parts with fine feature detail.

Applications

Clear PolyJet Resin (FC720) works well for prototypes that require smooth surface finish and high feature detail. Parts from this material can absorb paint or dye, be chrome plated, used as a master for silicone molds and have been used in investment casting. Clear PolyJet parts will have a semi-translucent appearance, which can be enhanced with sanding and buffing. Typical industries included toys, foot wear, architecture and any industry where feature detail and surface finish our required.

Available Properties
  • Base Resin Density
  • Ash
  • Hardness, Rockwell M
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Strength
  • Izod Impact, Notched
  • CTE, linear 20°C
  • CTE, linear 100°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。