Reliance Repol H020EG Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene H020EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H020EG is recommended for use in Extrusion & Blow Molding processes. It is an ideal material for making blow molded bottles, straws, ball pen refills, strappings, stationery items, sheets and thermoformed containers.Features: Good processing stabilityHigh melt strengthInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|