Reliance Repol H020SU Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene H020SU is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H020SU is recommended for Raffia Tapes used in making woven fabric for sacks, FIBC etc. for outdoor applications. Repol H020SU contains Hindered Amine Light Stabilizer (HALS) for protection against UV rays.Features: High tenacity in tapes Good processing stability High melt strengthInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|