Reliance Repol H030SG Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene H030SG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H030SG is recommended for Raffia Tapes used in making woven fabrics for sacking, carpet backing, industrial packaging and geotextile applications.Features: High tenacity in tapesConsistent processabilityLow "water carryover"Good color and processing stabilityInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|