Reliance Repol H080EG Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene H080EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H080EG is recommended for use in Cast Film Applications. Repol H080EG is an ideal material for textile overwraps, packaging of readymade garments, lamination films, snack food, twist wrap, grocery and general purpose packaging.Features: Consistent processability at high production ratesBetter downgaugingGood gloss and clarityGood heat seal strengthInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|