Reliance Repol H007EG Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene H007EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H007EG is recommended for use in extrusion and blow molding processes. It is an ideal material for making sheets and deep drawn thermoformed products, pipes, filter presses, strappings and blow molded bottles. Features: Good processing stability High melt strengthInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|