Reliance Repol R120MK Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene R120MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol R120MK is recommended for use in injection molding & stretch blow molding processes. It is an ideal material for attaining high clarity in housewares, syringes and ISBM products. Repol R120MK contains clarifier and antistatic agent that reduces static charge buildup on products. Features: Consistent processabilityGood claritySuperior mechanical propertiesLow static charge build-up and reduced dust pickupInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|