Reliance Repol C015EG Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol C015EG is recommended for use in blow molding and extrusion processes where high impact strength is required. It is an ideal material for making blow molded containers, sheets, automotive trims etc. Features: Consistent processabilityGood stiffness-impact balanceGood surface glossInformation provided by Reliance Industries
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|