Reliance Relene E52009 Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Relene E52009 is a High Density Polyethylene grade with low gel content, excellent orientation characteristics and negligible water carry-over. This grade is recommended for making raffia tapes and monofilaments with an excellent balance of high tenacity and good elongation. Information provided by Reliance Industries
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
|
|
|
|
| Property Data |