Reliance Relene E41003 Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial effluent as per IS 4984:1995, IS 14151:1995 and IS 14333:1996.Information provided by Reliance Industries
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
|
|
|
|