Reliance Relene B31101 Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Steel pipe coation base High Density Polyethylene resin. Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistance. Information provided by Reliance Industries
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Volume Resistivity
- Dielectric Constant
- Dissipation Factor
- Vicat Softening Point
|
|
|
|
| Property Data |