Reliance Relene C31101 Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Material Notes: Steel pipe coating High Density Polyethylene grade. Contains a minimum 2% of well dispersed carbon black.Characteristics:excellent weathering resistance, excellent processability, excellent adhesion. Information provided by Reliance Industries
| Available Properties |
- Density
- Water Absorption
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |