Reliance Reclair F19010 Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. This grade is good for heavy duty applications and liquid packaging. Characteristics: good toughness, good impact strength, and good tear resistance. Information provided by Reliance Industries
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Coefficient of Friction, Static
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|