Reliance Reclair F18020 Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, and films for lamination. Information provided by Reliance Industries
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
|
|
|
|