Reliance Reclair F22020 Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and blending with LDPE. Information provided by Reliance Industries
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Coefficient of Friction, Static
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
|
|
|
|