Resin Technology Group DPE110698-1 Two component Potting Compound
Subcategory: Adhesive; Thermoset
Material Notes: Resin Technology Group DPE110698-1 Two component Potting Compound Clear, fire retardant, low viscosity potting compound.
| Available Properties |
- Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Pot Life
|
|
|
|
| Property Data |