Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Mix ratio 100/50 by volume. TIGA 110EX-DP is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive, small potting and laminating applications where sparkling clarity and excellent structural, mechanical and electrical properties are required. This two-part adhesive exhibits good wetting, cures at room temperature and develops strong, low shrinkage, bonds to most materials including optical fibers, glass, ceramics, most metals and many rigid plastics. It has excellent dimensional stability over a wide temperature range. Fully cured TIGA 110EX-DP is a durable electrical insulator with good physical properties, plus resistance to water, weather, ozone and oxygen, petroleum solvents, lubricating oils, jet fuel, gasoline, alcohol, salt solutions, mild acids and alkalis and many other organic and inorganic compounds. Information provided by Resin Technology Group.
| Available Properties |
- Specific Gravity
- Viscosity
- Collected Volatile Condensable Material
- Hardness, Shore D
- Tensile Strength @ Break
- Shear Strength
- Dielectric Strength
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Softening Point
- Minimum Service Temperature, Air
- Glass Temperature
- Refractive Index
- Transmission, Visible
- Cure Time
- Pot Life
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|