Resin Technology Group CT-523LV Cationic UV Cure Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low outgassing polymer system capable of surviving exposure up to 200°C. Applications: Disk drive engineering products, non-acrylic UV bonding. No out gassing concerns. Use as conformal coat and/or wire tack. Opto-Electronic, Fillet-tacking and staking. Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers Recommended Aurora UV light sources: - Aurora 455-S 5x5 High Intensity Flood
- Aurora 461-S 1x6 High Intensity Beam
- Aurora 100-S Spot Light Guide
Information provided by Resin Technology Group.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength @ Break
- Shear Strength
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Transmission, Visible
- Color
- Composition
- Moisture Resistance
- Toxicity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|