Resirene® HF-666 General Purpose Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Calsak Corporation
Material Notes: Features:- High Flow
- Easy Processing
- High Productivity
- FDA Rating: 21 CFR 177.1640
- External Lubrication Available
Applications: - Medium Wall Applications
- Injection
- Toys
- Cassette Cases
Information provided by US distributor Calsak Corporation.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |