Resirene® READ 9500 Ignition Resistant Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: Calsak Corporation
Material Notes: Features:- High Flow
- Ignition Resistant
- No Pre-drying Required
- High Impact
- Colors Available
Applications: - Injection Molding
- Dark Colors
- TV Cabinets
- Electronic Equipment
Information provided by US distributor Calsak Corporation.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|