ChemRex® PRO 2000 Adhesive/Sealant

 

Subcategory: Adhesive; Elastomer, TS; Thermoset

Key Words: ChemRex, Inc.

Material Notes:
Typical applications of Pro 2000 adhesive/sealant include sealing around opening-doors, windows, air conditioners, skylights-in RV's, trailers and buses, bonding of vehicle trim and molding, waterproofing of roof and sidewall lap seams, bonding/sealing of joints constructed of prepainted metals, glass, aluminum and plastic composites, bonding of roof bows, waterproof and seal rivet seams, seal around corner and end moldings, glazing sealant on glass, aluminum, wood, concrete, fiberglass, and vinyl window systems, sealant for vinyl and aluminum.

Tack-free time is 25 minutes ± 3 minutes given the ASTM C 679 test method. Sag resistance is none given the ASTM C 2202 test method. Adhesion-in peel is 27 pli ± 3 pli given the ASTM C 794 test method. Bond durability is 25% total joint movement given the ASTM C 719 test method. Weathering after 500 hours indicates no change given the ASTM C 793 test method. No staining results from the ASTM 510 test method.

)

Information provided by ChemRex, Inc.

Available Properties
  • Density
  • Brookfield Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。