RheTech FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Subcategory: Polyolefin; Thermoplastic
Material Notes: Applications: - Cowl vent grilles
- Exterior components
- Bodyside moldings
Injection molding conditions reported in table. Information provided by RheTech Products.
| Available Properties |
- Specific Gravity
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Flexural Modulus
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Injection Pressure
- Hold Pressure
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|