Rhodia Technyl® A205F Nylon 66, EH0
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66; PA66
Material Notes: Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding. Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particularly suitable for the molding of long parts with thin wall sections, such as: cable tie, fasteners, and connectors. This product is available in natural, black and in colors on request. Glow wire test thick. 1,6 mm, IEC 695-2-1, 850°C. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|