Rhodia Technyl® A216 V30 Nylon 66, 30% Glass Fiber, EH0
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; PA66
Material Notes: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding. Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is used in automotive industry, manufacture of components of electrical tools, and transport and building. This product is available in natural, black and in a wide range of standard colors. Glow wire test thick. 1,6 mm, IEC 695-2-1, is 650°C. Glow wire test thick. 3,2 mm, IEC 695-2-1, is 750°C. Glow wire test thick. 1,6 mm: no flame, IEC 695-2-1, is 650°C. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Fill Speed
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|