Rhodia Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Polyamide 66; PA66
Material Notes: Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade in commonly used in the automotive industry of engine components, such as inlet manifolds, air ducts, engine cover, and various housing and liquid containers. This product is available in natural, black and grey. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|