Rhodia Technyl® A246M Nylon 66, Impact Grade, EH0
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66; PA66
Material Notes: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding. Technyl A 246m offers an excellent notched impact resistance at low temperatures making it suitable for sports and leisure applications. It is suitable for shoe soles, ski components, ski and surf bindings, as well as toy applications, such as the bumper of a remote-controlled car. This product is available in natural, white and black. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Fill Speed
- Injection Speed (cm3/sec)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|