Rhodia Technyl® B50H1 Nylon 66/6, Flame Retardant, EH0

 

Subcategory: Nylon; Thermoplastic; Nylon 6/66

Key Words: Polyamide 66/6; PA66/6; PA6/66; Nylon 6/66

Material Notes:
Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.

This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities and with good stiffness. It is particularly suitable for molding insulating parts for electrical components on board materials for use in tunnels, satisfying specification n°3 of the standard "Fire and Smoke" NF-F16102, and on components for electrical connections : junction blocks, terminal blocks, connectors.

This product is available in natural, black, and in colors on request.

Glow wire test thick. 1,6 mm, IEC 695-2-1, is 960°C. Glow wire test thick. 1,6 mm: no flame, IEC 695-2-1, is 650°C. Glow wire test thick. 0,8 mm: c<5s, IEC 695-2-1/HN60-E-02, is 960°C.

Information provided by Rhodia.

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Izod Impact Resistance
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Oxygen Index
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。