Rhodia Technyl® B50H1 Nylon 66/6, Flame Retardant, EH50
Subcategory: Nylon; Thermoplastic; Nylon 6/66
Key Words: Polyamide 66/6; PA66/6; PA6/66; Nylon 6/66
Material Notes: Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding. This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities and with good stiffness. It is particularly suitable for molding insulating parts for electrical components on board materials for use in tunnels, satisfying specification n°3 of the standard "Fire and Smoke" NF-F16102, and on components for electrical connections : junction blocks, terminal blocks, connectors. This product is available in natural, black, and in colors on request. Glow wire test thick. 1,6 mm: no flame, IEC 695-2-1, is 650°C. Glow wire test thick. 0,8 mm: c<5s, IEC 695-2-1/HN60-E-02, is 960°C. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|