Rhodia Technyl® C216 Nylon 6, 30% Glass Fiber, EH50
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6; PA6
Material Notes: Polyamide PA6, reinforced with 30% of glass fiber, for injection molding. It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. It is used in the automotive industry and electrical sectors. This product is available in colors on request. Information provided by Rhodia.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact Resistance
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Melting Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|