Rhodia Technyl® C216V30 30% Glass Filled Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Key Words: Polyamide 6; PA6
Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).
| Available Properties |
- Density
- Water Absorption
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Feed Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Fill Speed
- Injection Speed (cm3/sec)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|