Ritelok ECGEL Ethyl CA GEL Adhesive
Subcategory: Adhesive; Thermoset
Material Notes: Cyanoacrylate. Non-drip thixotropic gel, ideal for maximum gap filling. Non-drip, Excellent on porous surfaces, Allows post-assembly adjustment
Available Properties |
- Tensile Strength at Break
- Maximum Gap Fill
|
|
|
|