Ritelok PR100 Plastic & Rubber Adhesive
Subcategory: Adhesive; Thermoset
Material Notes: Cyanoacrylate. Medium strength plastic & rubber adhesive. For difficult to bond rubber & plastic. High bond strength, Medium viscosity, Fast cure