Ritelok PS67 Adhesive
Subcategory: Adhesive; Thermoset
Material Notes: Anaerobic. Pipe sealant, standard and stainless pipes. PS67 withstands temperatures from 65°F to 400°F (55°C-200°C), dismantled using normal tools
| Available Properties |
- Viscosity
- Maximum Service Temperature, Air
- Pressure Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|