1904B Glass Reinforced Electrical Encapsulation Grade Epoxy
Subcategory: Epoxy; Thermoset; Polymer
Close Analogs: Former Rogers & Vyncolit North America products are now manufactured by Sumitomo Bakelite North America.
Key Words: Rogers Epoxy
Material Notes: Data provided by the manufacturer, Rogers Molding Materials Division, 1998. Epoxy is the premier material for military firewall connectors.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Oxygen Index
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|