Degussa AG Rohacell® 110 Polymethacrylimide (PMI) Rigid Foam Sheet
Subcategory: Thermoset; Composite Core Material; Polymer
Close Analogs: This grade is not a part of the current Degussa product line.
Material Notes: ROHACELL 110 is a specialty grade which closes the gap between lower-density grades (31, 51, and 71) and the compacted, higher-density grades (P 170 and P 190). General ROHACELL Information: ROHACELL is a closed-cell rigid expanded plastic material for lightweight sandwich construction. It has excellent mechanical properties, high dimensional stability under heat, solvent resistance and, particularly at low temperature, a low thermal conductivity. The strength and moduli values are the highest are the highest for any foamed plastic in its density range. ROHACELL is manufactured by hot forming of methacrylic acid/methacrylonitrile copolymer sheets. During foaming this copolymer is converted to polymethacrylimide. Information supplied by Emkay Plastics, Ltd.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Modulus
- Shear Strength
- Maximum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|