Degussa AG Rohacell® 200EC-4 Electrically Conductive Grade Polymethacrylimide (PMI) Foam

 

Subcategory: Thermoset; Composite Core Material; Polymer

Material Notes:
Description: ROHACELL® is produced by thermal expansion of a co-polymer sheet of methacrylic acid and methacrylonitrile. During the foaming process the copolymer sheet is converted to PMI - PolyMethacrylImide. Alcohol is used as a blowing agent, thus ROHACELL® contains no fluorinated carbon hydrates and is halogen free. It has a very homogeneous cell structure and isotropic properties.

Specific Notes for this Material: ROHACELL® EC (= Electrically Conductive) is a closed-cell rigid foam plastic based on PMI (polymethacrylimide) which does not contain any CFCs. ROHACELL® EC is a specially developed material for applications were electro conductivity is desirable. Any commonly used manufacturing technique, such as autoclave, press molding and resin infusionb can be applied. Thermoformability is another advantage of ROHACELL® EC.

Information provided by degussa.

Available Properties
  • Density
  • Tensile Strength at Break
  • Modulus of Elasticity
  • Compressive Strength
  • Shear Strength
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。