Degussa AG Rohacell® 71 WF High Heat Grade Polymethacrylimide (PMI) Foam
Subcategory: Thermoset; Composite Core Material; Polymer
Material Notes: Description: ROHACELL® is produced by thermal expansion of a co-polymer sheet of methacrylic acid and methacrylonitrile. During the foaming process the copolymer sheet is converted to PMI - PolyMethacrylImide. Alcohol is used as a blowing agent, thus ROHACELL® contains no fluorinated carbon hydrates and is halogen free. It has a very homogeneous cell structure and isotropic properties. Specific Notes for this Material: ROHACELL® WF (= grade with increased heat distortion resistance) is a closed-cell rigid foam plastic based on PMI (polymethacrylimide) which does not contain any CFCs. ROHACELL® WF serves as a core material in advanced sandwich components used in aircraft and spacecraft construction. Curing temperature up to 180C (356F). Curing pressure up to 0.70 MPa (100 psi). Sandwich components using ROHACELL® WF as core material can be realized in a single work step (= cocuring). The structural components can be manufactured in an autoclave and by means of RTM. ROHACELL® WF is easy to shape. Thermoformability is another advantage of the core material. Information provided by degussa.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Shear Modulus
- Shear Strength
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|