Rosite® 4010ES SMC Thermoset Polyester, 22-25% Glass Reinforced
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Sheet Molding Compound; Oneida-Rostone Group (ORC Plastics)
Material Notes: Key Features: Business Machine Grade High strength, dimensional control, and surface smoothness. Information provided by Oneida-Rostone Group.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Flammability, UL94
|
|
|
|