Rosite® 6950D BMC Thermoset Polyester, 20% Glass Reinforced
Subcategory: Polyester, TS; Thermoset; Polymer
Key Words: Bulk Molding Compound; Oneida-Rostone Group (ORC Plastics)
Material Notes: Key Features: High Load and Elevated Temperature Applications Offers superior dimensional stability and creep resistance in high load or high temp uses. Information provided by Oneida-Rostone Group.