Spartech Royalite R60M Hi-Impact ABS/PVC Resin
Subcategory: Vinyl; ABS Polymer; Thermoplastic
Close Analogs: This grade is no longer part of the Spartech product line.
Key Words: Poly(Acrylonitrile-Butadiene-Styrene); Polyvinyl Chloride, Royalite Thermoplastics Division, Uniroyal Technology Corp.
Material Notes: Data provided by the manufacturer. This rigid, fire-rated, proprietary resin is specifically formulated to meet the requirements of the FAR 25.853 A flammability test. Primary applications are aircraft interior parts such as seat trim, trays and window surrounds.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|