| Available Properties |
- Specific Gravity
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Flexural Modulus
- Flexural Yield Strength
- Impact Test
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 1.8 MPa (264 psi)
- FAA 12 Second Vertical Burn
- FAA 60 Second Vertical Burn
- FAA Heat Release
- FAA Smoke Generation
- Flammability
|
|
|
|