RTP Company Grade 1607 Polyarylsulfone (PAS), Glass Fiber 40%
Subcategory: Polyarylsulfone; Thermoplastic; Polymer
Close Analogs: This product has been discontinued, please contact RTP Company regarding alternate grades.
Material Notes:
Data is for injection molded specimens and was provided by the manufacturer, RTP Company.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- K (wear) Factor
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|