Sawbones® E-Glass-Filled Epoxy Cylinders
Subcategory: Epoxy; Thermoset; Composite Core Material; Polymer
Material Notes: Primary Use E-glass-filled epoxy cylinders are primarily used as an alternative test medium to human cortical bone.
Description They are a mixture of short e-glass fibers and epoxy resin that has been pressure molded into hollow cylinders. They can be filled with rigid or cellular foam upon request for an additional charge. Information provided by Sawbones.