INEOS HDPE HP54-60-FLK
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: Innovene is a wholly owned subsidiary of BP Group.
Key Words: For plastic wood composites
Material Notes: Description: Fortiflex® HDPE HP54-60-FLK is a high density polyethylene copolymer flake which contains no additives and is not pelletized. It is designed for use in the plastic wood composite market. Information from manufacturer data sheet.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|